增材制造钛合金等效弹性张量的细观力学建模与实验研究
|
|
谭若涵, 宋永锋, 陈超, 李丹, 成庶, 李雄兵
|
Mesomechanical Modeling and Experimental Study of Effective Elastic Tensors in Additively Manufactured Titanium Alloys
|
|
TAN Ruohan, SONG Yongfeng, CHEN Chao, LI Dan, CHENG Shu, LI Xiongbing
|
|
表6 基于MMT模型和超声实验获得的AM Ti-6Al-4V试块 Ceff及其MAPE和EC
|
Table 6 , , , , , and of AM Ti-6Al-4V alloy by MMT method and ultrasonic test, along with its MAPE and EC
|
|
| Sample | Indicator |
GPa |
GPa |
GPa |
GPa |
GPa |
GPa | MAPE % | EC % |
|---|
| A | V-MMT | 152.60 | 163.09 | 157.36 | 48.42 | 40.50 | 44.06 | 9.47 | 94.35 | | Ultrasonic | 143.68 | 143.23 | 136.92 | 44.11 | 44.98 | 43.18 | | | | B | V-MMT | 165.65 | 175.67 | 170.34 | 51.25 | 43.31 | 46.97 | 4.45 | 98.49 | | Ultrasonic | 169.43 | 169.60 | 171.60 | 47.09 | 46.79 | 45.21 | | |
|
|
|