水平集法模拟GH4706合金动态再结晶过程 |
| 郑德宇, 夏玉峰, 曾扬, 周杰 |
|
Dynamic Recrystallization Process Simulation of GH4706 Alloy by Level-Set Method |
| ZHENG Deyu, XIA Yufeng, ZENG Yang, ZHOU Jie |
| 图3 晶粒形核过程示意图 |
| Fig.3 Schematic of grain nucleation process (ρ—dislocation density, ρcr—critical dislocation density, L—critical nucleation distance) |
|