水平集法模拟GH4706合金动态再结晶过程 |
| 郑德宇, 夏玉峰, 曾扬, 周杰 |
|
Dynamic Recrystallization Process Simulation of GH4706 Alloy by Level-Set Method |
| ZHENG Deyu, XIA Yufeng, ZENG Yang, ZHOU Jie |
| 图2 采用水平集函数定义晶界 |
| Fig.2 Definition of grain boundaries using level-set functions (Ψ represents level-set function; Ψ1, Ψ2, and Ψ3 represent level set functions for Grain 1, Grain 2, and Grain 3, respectively) |
|