激光熔覆Si增强MoNiCr合金涂层及其高温摩擦学性能
尤世泉, 崔功军, 杨荣乾, 刘宇嵩, 冯小刚, 寇子明

High-Temperature Tribological Performance of Laser Clad MoNiCr Alloy Coatings Reinforced by Si
YOU Shiquan, CUI Gongjun, YANG Rongqian, LIU Yusong, FENG Xiaogang, KOU Ziming
表2 图3中标记区域的EDS结果 (mass fraction / %)
Table 2 EDS results of the marked regions in Fig.3
RegionCSiCrNiMo
A2.76013.5439.8143.89
B1.7509.2123.8165.23
C2.561.2812.5340.2143.42
D1.601.299.5524.3663.20