激光熔覆Si增强MoNiCr合金涂层及其高温摩擦学性能 |
| 尤世泉, 崔功军, 杨荣乾, 刘宇嵩, 冯小刚, 寇子明 |
|
High-Temperature Tribological Performance of Laser Clad MoNiCr Alloy Coatings Reinforced by Si |
| YOU Shiquan, CUI Gongjun, YANG Rongqian, LIU Yusong, FENG Xiaogang, KOU Ziming |
| 图3 MoNiCr和MoNiCrSi涂层横截面不同位置的背散射电子(BSE)像 |
| Fig.3 Cross-sectional backscattered electron (BSE) images of MoNiCr (a, b) and MoNiCrSi (c, d) coatings at different areas (a, c) close to the interface (b, d) close to the surface |
|