斜纹碳布缝合织物结构增强铝基复合材料的高温拉伸及断裂行为
吴志勇, 邵徽凡, 蔡长春, 曾敏, 王振军, 王艳丽, 陈雷, 熊博文

Tensile and Fracture Behaviors of Stitched Twill Carbon Fabric Structure Reinforced Aluminum Matrix Composites at Elevated Temperature
WU Zhiyong, SHAO Huifan, CAI Changchun, ZENG Min, WANG Zhenjun, WANG Yanli, CHEN Lei, XIONG Bowen
表5 铝基复合材料高温拉伸力学性能的实验与计算结果
Table 5 High-temperature tensile properties obtained from the experiment and simulation

Data type

Elastic

modulus

GPa

Ultimate

strength

MPa

Elongation

%

Calculation error / %7.171.943.79
Experimental value103.20621.600.819
Numerical value110.60633.640.850