GH3230合金薄板填丝钨极氩弧焊接头的组织稳定性 |
| 张天昊, 鞠泉, 蒙肇斌, 王浩, 胡本芙 |
|
Microstructural Stability in Tungsten Argon-Arc Welded Joint of GH3230 Superalloy Plate |
| ZHANG Tianhao, JU Quan, MENG Zhaobin, WANG Hao, HU Benfu |
| 图9 GH3230合金填丝钨极氩弧焊接薄板经不同温度热暴露2000 h后不同区域M23C6型碳化物的平均尺寸 |
| Fig.9 Average sizes of M23C6 carbides in different regions of GH3230 alloy weld plate after thermal exposure at different temperatures for 2000 h |
|