Similarities and Differences of Microstructure and Mechanical Properties Between High γ' Content Powder and Wrought Superalloys
WANG Hongying, YAO Zhihao, LI Dayu, GUO Jing, YAO Kaijun, DONG Jianxin
图8 FGH4720Li和GH4720Li合金中的晶粒取向分布图及晶粒尺寸分布图
Fig.8 Grain orientation distribution maps (a1-f1) and grain size distributions (a2-f2) of FGH4720Li and GH4720Li alloys (G—grain grade)
(a1, a2) FGH-1 (b1, b2) FGH-2 (c1, c2) FGH-3 (d1, d2) GH-1 (e1, e2) GH-2 (f1, f2) GH-3