V分布特性对新型980 MPa级海工特厚板用钢淬透性的影响 |
| 傅万堂, 王薇, 任利国, 白兴红, 吕知清, 李荣斌, 刘浩楠, 齐建军 |
|
Effect of V Distribution Characteristics on the Hardenability of a Novel 980 MPa Grade Extra-Thick Steel Plate for Marine Engineering |
| FU Wantang, WANG Wei, REN Liguo, BAI Xinghong, LV Zhiqing, LI Rongbin, LIU Haonan, QI Jianjun |
| 图3 910和850 ℃奥氏体化后距淬火端不同位置处实验用钢显微组织的OM像 |
| Fig.3 OM images of test steel at the distances of 5 mm (a, d), 30 mm (b, e), and 55 mm (c, f) from the quenched end after austenitizing at 910 oC (a-c) and 850 oC (d-f) |
|