Zr ODS FeCrAl合金在550Pb-Bi熔液中的腐蚀行为
张晓晨, 李静, 李长记, 熊良银, 刘实

Corrosion Behavior of ODS FeCrAl Alloys Containing Zr Exposed to Lead-Bismuth Eutectic at 550 oC
ZHANG Xiaochen, LI Jing, LI Changji, XIONG Liangyin, LIU Shi
表1 氧化物弥散强化(ODS) FeCrAl合金的化学成分 (mass fraction / %)
Table 1 Chemical compositions of oxide dispersion strengthened (ODS) FeCrAl alloys
AlloyCrWAlTiZrYOEx.OFe
CAZ-113.481.695.30-0.310.360.120.023Bal.
CAZ-213.581.695.28-0.310.360.240.143Bal.
CAZ-313.511.705.230.350.300.370.230.130Bal.
CAZ-413.991.814.110.330.280.350.100.006Bal.
CAZ-513.991.814.180.350.290.340.230.138Bal.