含Zr ODS FeCrAl合金在550 ℃ Pb-Bi熔液中的腐蚀行为 |
| 张晓晨, 李静, 李长记, 熊良银, 刘实 |
|
Corrosion Behavior of ODS FeCrAl Alloys Containing Zr Exposed to Lead-Bismuth Eutectic at 550 oC |
| ZHANG Xiaochen, LI Jing, LI Changji, XIONG Liangyin, LIU Shi |
| 图13 5种合金疖状腐蚀产物的表面平均横向尺寸和平均厚度及数密度 |
| Fig.13 Statistical results of average surface transverse dimension and average thickness (a), number density (b) for oxide nodules on the five alloys |
|