Zr ODS FeCrAl合金在550Pb-Bi熔液中的腐蚀行为
张晓晨, 李静, 李长记, 熊良银, 刘实

Corrosion Behavior of ODS FeCrAl Alloys Containing Zr Exposed to Lead-Bismuth Eutectic at 550 oC
ZHANG Xiaochen, LI Jing, LI Changji, XIONG Liangyin, LIU Shi
图9 经550 ℃、饱和氧LBE腐蚀10000 h后CAZ-5合金表面疖状腐蚀产物截面的EPMA元素面扫描结果
Fig.9 EPMA elemental mapping results of cross-section of oxide nodules on CAZ-5 alloy exposed to oxygen-saturated LBE at 550 oC for 10000 h