含Zr ODS FeCrAl合金在550 ℃ Pb-Bi熔液中的腐蚀行为 |
| 张晓晨, 李静, 李长记, 熊良银, 刘实 |
|
Corrosion Behavior of ODS FeCrAl Alloys Containing Zr Exposed to Lead-Bismuth Eutectic at 550 oC |
| ZHANG Xiaochen, LI Jing, LI Changji, XIONG Liangyin, LIU Shi |
| 图8 经550 ℃、饱和氧LBE腐蚀10000 h后CAZ-3和CAZ-5合金氧化产物表面与截面形貌的SEM像 |
| Fig.8 Surface (a, c) and cross-sectional (b, d) SEM images of oxide products on CAZ-3 (a, b) and CAZ-5 (c, d) alloys exposed to oxygen-saturated LBE at 550 oC for 10000 h |
|