聚变用低活化9Cr-ODS钢在高温高压水中的腐蚀行为及机理
付海阳, 张家榕, 李尧志, 王旗涛, 李新乐, 严伟, 单以银, 李艳芬

Corrosion Behavior and Mechanism of Low Activation 9Cr-ODS Steel in High Temperature and High Pressure Water Environment for the Application in Fusion Reactors
FU Haiyang, ZHANG Jiarong, LI Yaozhi, WANG Qitao, LI Xinle, YAN Wei, SHAN Yiyin, LI Yanfen
图14 9Cr-ODS钢在静态、动态高温高压水中腐蚀过程的示意图
Fig.14 Schematics of corrosion process of 9Cr-ODS steel in static and dynamic high temperature and high pressure water
(a) early stage of corrosion (b) static (c) dynamic