聚变用低活化9Cr-ODS钢在高温高压水中的腐蚀行为及机理 |
| 付海阳, 张家榕, 李尧志, 王旗涛, 李新乐, 严伟, 单以银, 李艳芬 |
|
Corrosion Behavior and Mechanism of Low Activation 9Cr-ODS Steel in High Temperature and High Pressure Water Environment for the Application in Fusion Reactors |
| FU Haiyang, ZHANG Jiarong, LI Yaozhi, WANG Qitao, LI Xinle, YAN Wei, SHAN Yiyin, LI Yanfen |
| 图7 9Cr-ODS和CLAM钢在静态和动态高温高压水中腐蚀1000 h后外表面Fe的详细XPS |
| Fig.7 Detailed XPS of Fe on the outer surface of 9Cr-ODS (a, c) and CLAM (b, d) steels after corrosion in static (a, b) and dynamic (c, d) high temperature and high pressure water for 1000 h |
|