聚变用低活化9Cr-ODS钢在高温高压水中的腐蚀行为及机理  | 
		
| 付海阳, 张家榕, 李尧志, 王旗涛, 李新乐, 严伟, 单以银, 李艳芬 | 
| 
				 Corrosion Behavior and Mechanism of Low Activation 9Cr-ODS Steel in High Temperature and High Pressure Water Environment for the Application in Fusion Reactors  | 
		
| FU Haiyang, ZHANG Jiarong, LI Yaozhi, WANG Qitao, LI Xinle, YAN Wei, SHAN Yiyin, LI Yanfen | 
| 图5 静态条件下腐蚀不同时间后9Cr-ODS和CLAM钢表面腐蚀产物的SEM像 | 
	
| Fig.5 Surface corrosion product SEM images of 9Cr-ODS (a-c) and CLAM (d-f) steels after corrosion in static condition for 200 h (a, d), 500 h (b, e), and 1000 h (c, f) | 
	
			 
		 |