聚变用低活化9Cr-ODS钢在高温高压水中的腐蚀行为及机理 |
| 付海阳, 张家榕, 李尧志, 王旗涛, 李新乐, 严伟, 单以银, 李艳芬 |
|
Corrosion Behavior and Mechanism of Low Activation 9Cr-ODS Steel in High Temperature and High Pressure Water Environment for the Application in Fusion Reactors |
| FU Haiyang, ZHANG Jiarong, LI Yaozhi, WANG Qitao, LI Xinle, YAN Wei, SHAN Yiyin, LI Yanfen |
| 图3 9Cr-ODS和CLAM钢在静态和动态高温高压水中的氧化增重曲线 |
| Fig.3 Oxidation mass gain (ΔW) curves of 9Cr-ODS and CLAM steels in static and dynamic high temperature and high pressure water (t—time) |
|