Prediction of Damage and Hot Forming Limit of TA32 Titanium Alloy Based on Crystal Plasticity Model
FAN Ronglei, CHEN Minghe, WU Dipeng, WU Yong
表1 钛合金中α相和β相的物理参数[23,24]
Table 1 Physical parameters of α and β phases in titanium alloy[23,24]
Phaseμ0 / GPaTM / KTMμ0dμdTElastic constant at room temperature / GPa
C11C12C13C33C44
α43.61933-1.2141.076.957.9163.048.7
β20.51933-0.5135.0113.0--54.9