基于晶体塑性模型预测TA32钛合金损伤及高温成形极限 |
范荣磊, 陈明和, 吴迪鹏, 武永 |
Prediction of Damage and Hot Forming Limit of TA32 Titanium Alloy Based on Crystal Plasticity Model |
FAN Ronglei, CHEN Minghe, WU Dipeng, WU Yong |
图11 不同路径下达到最小极限应变时的凹槽临界初始倾角 |
Fig.11 Critical initial incline angles of groove (θ0) at the minimum limit strain under different strain paths (Insets are M-K models with corresponding initial inclination angles) |
![]() |