基于晶体塑性模型预测TA32钛合金损伤及高温成形极限 |
范荣磊, 陈明和, 吴迪鹏, 武永 |
Prediction of Damage and Hot Forming Limit of TA32 Titanium Alloy Based on Crystal Plasticity Model |
FAN Ronglei, CHEN Minghe, WU Dipeng, WU Yong |
图6 CPFE模型单轴拉伸实验结果与模拟结果对比及云图 |
Fig.6 Uniaxial tensile simulation results from CPFE model (a) stress-strain curves of experimental and simulated results (b, c) stress nephogram (b) and strain nephogram (c) of RVE deformed to equivalent strain 0.3 at a strain rate of 0.01 s-1 |
![]() |