5182-O铝合金屈服演化行为表征及晶体塑性模拟 |
尚宏春, 田中旺, 牛兰杰, 范晨阳, 张哲伟, 娄燕山 |
Yield Evolution Behavior Characterization and Crystal Plasticity Simulation for 5182-O Aluminum Alloy |
SHANG Hongchun, TIAN Zhongwang, NIU Lanjie, FAN Chenyang, ZHANG Zhewei, LOU Yanshan |
图17 单向压缩、0.2应变条件下5182-O铝合金的累积塑性滑移云图和应变为0.0~0.2时剖面图 |
Fig.17 Contour maps of cumulative plastic slips of 5182-O aluminum alloy at 0.2 strain under uniaxial compression (a-e) and cross-sectinal profile at strains of 0.0-0.2 (f) (a) Cube texture (b) Goss texture (c) Brass texture (d) Copper texture (e) S texture |
![]() |