5182-O铝合金屈服演化行为表征及晶体塑性模拟
尚宏春, 田中旺, 牛兰杰, 范晨阳, 张哲伟, 娄燕山

Yield Evolution Behavior Characterization and Crystal Plasticity Simulation for 5182-O Aluminum Alloy
SHANG Hongchun, TIAN Zhongwang, NIU Lanjie, FAN Chenyang, ZHANG Zhewei, LOU Yanshan
图15 RVE模型的宏观应力状态
Fig.15 Macroscopic stress states of RVE model (B1-,B1+,B2+, B3+—periodic boundary conditions; Σ11, Σ22, Σ33—diagonal components of the macroscopic Cauchy stress tensors)