5182-O铝合金屈服演化行为表征及晶体塑性模拟
尚宏春, 田中旺, 牛兰杰, 范晨阳, 张哲伟, 娄燕山

Yield Evolution Behavior Characterization and Crystal Plasticity Simulation for 5182-O Aluminum Alloy
SHANG Hongchun, TIAN Zhongwang, NIU Lanjie, FAN Chenyang, ZHANG Zhewei, LOU Yanshan
图13 5182-O铝合金初始取向及晶粒数量为400和500晶时取向织构的极图
Fig.13 Pole figures of textures for 5182-O aluminum alloys
(a) initial orientation (b) 400 grain orientation (c) 500 grain orientation