5182-O铝合金屈服演化行为表征及晶体塑性模拟 |
尚宏春, 田中旺, 牛兰杰, 范晨阳, 张哲伟, 娄燕山 |
Yield Evolution Behavior Characterization and Crystal Plasticity Simulation for 5182-O Aluminum Alloy |
SHANG Hongchun, TIAN Zhongwang, NIU Lanjie, FAN Chenyang, ZHANG Zhewei, LOU Yanshan |
图12 1/8代表性体积单元(RVE)有限元网格模型 |
Fig.12 Finite element mesh model of 1/8 representative volume element (RVE) |
![]() |