5182-O铝合金屈服演化行为表征及晶体塑性模拟 |
| 尚宏春, 田中旺, 牛兰杰, 范晨阳, 张哲伟, 娄燕山 |
|
Yield Evolution Behavior Characterization and Crystal Plasticity Simulation for 5182-O Aluminum Alloy |
| SHANG Hongchun, TIAN Zhongwang, NIU Lanjie, FAN Chenyang, ZHANG Zhewei, LOU Yanshan |
| 图11 5182-O铝合金初态取向织构的EBSD分析 |
| Fig.11 Inverse pole figure (a) and volume fraction distributions (b) of initial orientation texture for 5182-O aluminum alloy |
|