5182-O铝合金屈服演化行为表征及晶体塑性模拟 |
尚宏春, 田中旺, 牛兰杰, 范晨阳, 张哲伟, 娄燕山 |
Yield Evolution Behavior Characterization and Crystal Plasticity Simulation for 5182-O Aluminum Alloy |
SHANG Hongchun, TIAN Zhongwang, NIU Lanjie, FAN Chenyang, ZHANG Zhewei, LOU Yanshan |
图 7 不同等效塑性应变下5182-O铝合金的3D屈服面和实验结果对比 |
Fig.7 Comparisons of 3D yield surfaces and experimental results of 5182-O aluminum alloys under different (a) |
![]() |