5182-O铝合金屈服演化行为表征及晶体塑性模拟 |
| 尚宏春, 田中旺, 牛兰杰, 范晨阳, 张哲伟, 娄燕山 |
|
Yield Evolution Behavior Characterization and Crystal Plasticity Simulation for 5182-O Aluminum Alloy |
| SHANG Hongchun, TIAN Zhongwang, NIU Lanjie, FAN Chenyang, ZHANG Zhewei, LOU Yanshan |
| 图 5 不同试样断口形貌的SEM像 |
| Fig.5 SEM images showing fracture morphologies of UT0 (a), PST0 (b), and SS0 (c) specimens |
|