双非晶相铁基复合涂层的腐蚀与磨损行为 |
臧勃林, 杨延格, 曹京宜, 徐锋锋, 姚海华, 周正 |
Corrosion and Wear Behaviors of Fe-Based Composite Coating with Dual Amorphous Phases |
ZANG Bolin, YANG Yange, CAO Jingyi, XU Fengfeng, YAO Haihua, ZHOU Zheng |
图7 铁基非晶涂层磨痕形貌及测量结果 |
Fig.7 3D morphologies (unit: μm) (a, c, e) and measured results (b, d, f) of the wear tracks of Fe-based amorphous coatings (a, b) FN (c, d) FM (e, f) FH |
![]() |