双非晶相铁基复合涂层的腐蚀与磨损行为 |
臧勃林, 杨延格, 曹京宜, 徐锋锋, 姚海华, 周正 |
Corrosion and Wear Behaviors of Fe-Based Composite Coating with Dual Amorphous Phases |
ZANG Bolin, YANG Yange, CAO Jingyi, XU Fengfeng, YAO Haihua, ZHOU Zheng |
图5 铁基非晶涂层在3.5%NaCl溶液中的Nyquist图、Bode图和等效电路 |
Fig.5 Nyquist (a) and Bode (b) plots of the Fe-based amorphous coatings in 3.5%NaCl solution (Inset in Fig.5a is the equivalent circuit of coatings for EIS fitting. Z'—real part of the impedance, Z''—imaginary part of the impedance, |Z|—modulus of impedance, Rs—solution resistance, Rt—charge transfer resistance,CPE-dl—constant phase angle element related to electric double layer capacity, CPE-f—constant phase angle element related to passive film capacity, Rf—passive film resistance) |
![]() |