双非晶相铁基复合涂层的腐蚀与磨损行为 |
| 臧勃林, 杨延格, 曹京宜, 徐锋锋, 姚海华, 周正 |
|
Corrosion and Wear Behaviors of Fe-Based Composite Coating with Dual Amorphous Phases |
| ZANG Bolin, YANG Yange, CAO Jingyi, XU Fengfeng, YAO Haihua, ZHOU Zheng |
| 图3 铁基非晶涂层微区TEM明场像及选区电子衍射(SAED)花样 |
| Fig.3 Bright-field TEM images and selected area electron diffraction (SAED) patterns (insets) of FN (a), FM (b), and FH (c) coatings |
|