双非晶相铁基复合涂层的腐蚀与磨损行为 |
| 臧勃林, 杨延格, 曹京宜, 徐锋锋, 姚海华, 周正 |
|
Corrosion and Wear Behaviors of Fe-Based Composite Coating with Dual Amorphous Phases |
| ZANG Bolin, YANG Yange, CAO Jingyi, XU Fengfeng, YAO Haihua, ZHOU Zheng |
| 图1 铁基非晶涂层的XRD谱 |
| Fig.1 XRD spectra of the Fe-based amorphous coatings (FN—Fe59Cr12Nb5B20Si4, FM—Fe48Cr15Mo14-C15B6Y2, FH—50%FN + 50%FM (mass fraction)) |
|