20CrMnTi齿轮钢表面FeS涂层的干摩擦性能 |
||||||||||||||||||||
| 张国涛, 马镇, 李其龙, 李聪敏, 马涛, 马少波, 尹延国 | ||||||||||||||||||||
|
Dry Friction Performance of FeS Coating on the Surface of 20CrMnTi Gear Steel |
||||||||||||||||||||
| ZHANG Guotao, MA Zhen, LI Qilong, LI Congmin, MA Tao, MA Shaobo, YIN Yanguo | ||||||||||||||||||||
| 表3 不同转速条件1#试样磨损面部分元素含量 (mass fraction / %) |
||||||||||||||||||||
| Table 3 Contents of some elements on the wear surface of 1# sample at different speed conditions |
||||||||||||||||||||
|
||||||||||||||||||||