20CrMnTi齿轮钢表面FeS涂层的干摩擦性能
张国涛, 马镇, 李其龙, 李聪敏, 马涛, 马少波, 尹延国

Dry Friction Performance of FeS Coating on the Surface of 20CrMnTi Gear Steel
ZHANG Guotao, MA Zhen, LI Qilong, LI Congmin, MA Tao, MA Shaobo, YIN Yanguo
图6 0#、1#试样在不同工况下的摩擦系数曲线及其平均摩擦系数
Fig.6 Friction coefficient curves of 0# and 1# samples under different working conditions and their average friction coefficients
(a) different loading conditions (b) different speed conditions
(c) friction coefficient of 0# sample (d) average friction coefficient