20CrMnTi齿轮钢表面FeS涂层的干摩擦性能 |
张国涛, 马镇, 李其龙, 李聪敏, 马涛, 马少波, 尹延国 |
Dry Friction Performance of FeS Coating on the Surface of 20CrMnTi Gear Steel |
ZHANG Guotao, MA Zhen, LI Qilong, LI Congmin, MA Tao, MA Shaobo, YIN Yanguo |
图2 改性前后试样(分别记为0#和1#试样)的宏观形貌 |
Fig.2 Macroscopic morphology of the sample before and after the chemical reaction (marked as 0# and 1# samples, respectively) |
![]() |