20CrMnTi齿轮钢表面FeS涂层的干摩擦性能 |
| 张国涛, 马镇, 李其龙, 李聪敏, 马涛, 马少波, 尹延国 |
|
Dry Friction Performance of FeS Coating on the Surface of 20CrMnTi Gear Steel |
| ZHANG Guotao, MA Zhen, LI Qilong, LI Congmin, MA Tao, MA Shaobo, YIN Yanguo |
| 图1 摩擦实验示意图 |
| Fig.1 Schematic of friction experiment (V—velocity) |
|