耐热钢及搪瓷涂层在600 ℃高温CO2 气氛中的腐蚀行为 |
李雪, 喻政, 解志文, 王金龙, 陈明辉, 王福会 |
Corrosion Behavior of Heat-Resistant Steels and Its Enamel Coatings in CO2 Atmosphere at 600 oC |
LI Xue, YU Zheng, XIE Zhiwen, WANG Jinlong, CHEN Minghui, WANG Fuhui |
图9 4种试样在600 ℃、CO2气氛中腐蚀500 h后的截面OM像 |
Fig.9 Cross-sectional OM images of the four samples after corrosion at 600 oC in CO2 for 500 h (a) T92 (b) 316L (c) T92-TC (d) 316L-TC |
![]() |