耐热钢及搪瓷涂层在600 ℃高温CO2 气氛中的腐蚀行为 |
| 李雪, 喻政, 解志文, 王金龙, 陈明辉, 王福会 |
|
Corrosion Behavior of Heat-Resistant Steels and Its Enamel Coatings in CO2 Atmosphere at 600 oC |
| LI Xue, YU Zheng, XIE Zhiwen, WANG Jinlong, CHEN Minghui, WANG Fuhui |
| 图3 T92和316L钢在600 ℃、CO2气氛中腐蚀500 h后的表面SEM像 |
| Fig.3 Low (a, b) and high (c, d) magnified surface SEM images of T92 (a, c) and 316L (b, d) steels after corrosion at 600 oC in CO2 for 500 h |
|