耐热钢及搪瓷涂层在600 ℃高温CO2 气氛中的腐蚀行为 |
| 李雪, 喻政, 解志文, 王金龙, 陈明辉, 王福会 |
|
Corrosion Behavior of Heat-Resistant Steels and Its Enamel Coatings in CO2 Atmosphere at 600 oC |
| LI Xue, YU Zheng, XIE Zhiwen, WANG Jinlong, CHEN Minghui, WANG Fuhui |
| 图2 T92和316L钢在600 ℃、CO2气氛中腐蚀500 h前后的XRD谱 |
| Fig.2 XRD spectra of T92 (a) and 316L (b) steels before and after corrosion at 600 oC in CO2 for 500 h (I represents sample after corrosion, II represents sample after corrosion with 1/2 scale ground off, III represents sample after corrosion with scale ground off) |
|