耐热钢及搪瓷涂层在600 ℃高温CO2 气氛中的腐蚀行为 |
| 李雪, 喻政, 解志文, 王金龙, 陈明辉, 王福会 |
|
Corrosion Behavior of Heat-Resistant Steels and Its Enamel Coatings in CO2 Atmosphere at 600 oC |
| LI Xue, YU Zheng, XIE Zhiwen, WANG Jinlong, CHEN Minghui, WANG Fuhui |
| 图1 4种试样在600 ℃、CO2气氛中腐蚀500 h的动力学曲线 |
| Fig.1 Kinetic curves of the four samples after corrosion at 600 oC in CO2 for 500 h (Inset shows the locally high magnified curves. 316L-TC represent 316L austenitic steel with enamel coating, T92-TC represents T92 ferritic steel with enamal coating) |
|