喷射成形工艺对M3高速钢碳化物特征及力学性能的影响 |
| 刘继浩, 迟宏宵, 武会宾, 马党参, 周健, 谷金波 |
|
Influence of Spray Forming Process on Carbide Characteristics and Mechanical Properties of M3 High-Speed Steel |
| LIU Jihao, CHI Hongxiao, WU Huibin, MA Dangshen, ZHOU Jian, GU Jinbo |
| 图16 Thermol-Calc软件中Equilibrium模型的碳化物析出计算结果 |
| Fig.16 Calculation results of carbide precipitation obtained by Equilibrium model in Thermol-Calc software |
|