喷射成形工艺对M3高速钢碳化物特征及力学性能的影响 |
| 刘继浩, 迟宏宵, 武会宾, 马党参, 周健, 谷金波 |
|
Influence of Spray Forming Process on Carbide Characteristics and Mechanical Properties of M3 High-Speed Steel |
| LIU Jihao, CHI Hongxiao, WU Huibin, MA Dangshen, ZHOU Jian, GU Jinbo |
| 图7 ESR-M3高速钢纵向试样冲击断口形貌的SEM像 |
| Fig.7 SEM images of impact fracture of longitudinal ESR-M3 high-speed steel specimen (a) macro fracture morphology (b) micro fracture morphology (c) characteristics of quasi cleavage fracture morphology (d) cracks propagate along carbides (e) large scale carbide fracture |
|