γ-TiAl合金在700 ℃空气中的长时高温氧化行为和组织演变
周志春, 刘仁慈, 张建达, 杨超, 崔玉友, 杨锐

Long-Term Oxidation Behavior and Microstructural Evolution of γ-TiAl Alloys at 700 oC in Air
ZHOU Zhichun, LIU Renci, ZHANG Jianda, YANG Chao, CUI Yuyou, YANG Rui
表2 45XD和4822合金样品表面氧化产物化学成分分析 (atomic fraction / %)
Table 2 Chemical composition of oxides on the surface of 45XD and 4822 alloy specimens
AlloyPositionOAlTiNbMnCr
45XD153.9521.1123.820.710.41-
264.5316.8617.900.370.34-
368.2814.6216.650.280.17-
4822456.8019.2522.300.85-0.80
569.610.4229.750.19-0.03
658.8822.7017.610.45-0.36
772.720.4026.680.16-0.04