横向弱磁场对镍基高温合金发散双晶竞争生长行为的影响
谢信亮, 周丽萍, 余建波, 玄伟东, 陈超越, 王江, 任忠鸣

Effect of Weak Transverse Magnetic Field on the Competitive Grain Growth of Ni-Based Superalloy with Divergent Bi-Crystals
XIE Xinliang, ZHOU Liping, YU Jianbo, XUAN Weidong, CHEN Chaoyue, WANG Jiang, REN Zhongming
图8 磁场强度为0、0.1和0.7 T时发散双晶中θGB随拉速的变化
Fig.8 θGB of the divergent bi-crystals as a function of withdrawal rate under the magnetic fields of 0, 0.1, and 0.7 T