316L激光粉末床熔覆IN718偏析带形成过程的模拟 |
| 沈盟凯, 董太宁, 葛鸿浩, 石新升, 张群莉, 刘云峰, 姚建华 |
|
Simulation of the Formation Mechanism of Segregation Bands During IN718 Cladding on 316L Using Laser Powder Bed Fusion |
| SHEN Mengkai, DONG Taining, GE Honghao, SHI Xinsheng, ZHANG Qunli, LIU Yunfeng, YAO Jianhua |
| 图8 t = 1.17 s时Fe元素的分布云图 |
| Fig.8 Distribution nephogram of Fe element at t = 1.17 s |
|