热压温度对TC4合金扩散连接区组织与性能的影响 |
| 张洺川, 徐勤思, 刘意, 蔡雨升, 牟义强, 任德春, 吉海宾, 雷家峰 |
|
Effect of Hot-Pressing Temperature on the Microstructure and Properties of the Diffusion-Bonded Region of TC4 Alloy |
| ZHANG Mingchuan, XU Qinsi, LIU Yi, CAI Yusheng, MU Yiqiang, REN Dechun, JI Haibin, LEI Jiafeng |
| 图9 扩散连接区经热处理后显微组织的SEM像 |
| Fig.9 SEM images of diffusion bonding regions after heat treatment (970 oC, 2 h, air cooling) (a) sample 1# (b) sample 2# (c) sample 3# |
|