B含量调控Fe98.5 -x B x Cu1.5 纳米晶合金组织结构和磁性能 |
| 朱春健, 李艳辉, 朱正旺, 吴立成, 张海峰, 张伟 |
|
Regulation of Structure and Magnetic Properties of Fe98.5 -x B x Cu1.5 Nanocrystalline Alloys Based on B Content |
| ZHU Chunjian, LI Yanhui, ZHU Zhengwang, WU Licheng, ZHANG Haifeng, ZHANG Wei |
| 图3 Fe98.5 - x B x Cu1.5快淬合金的TEM明场像和HRTEM像 |
| Fig.3 Bright-field TEM images and corresponding SAED patterns and grain size distributions with normal fitting (insets) (a, c, e) and HRTEM images (b, d, f) of melt-spun Fe98.5 - x B x Cu1.5 alloys with x = 12 (a, b), x = 15 (c, d), and x = 18 (e, f) ( |
|