B含量调控Fe98.5 -x B x Cu1.5 纳米晶合金组织结构和磁性能 |
| 朱春健, 李艳辉, 朱正旺, 吴立成, 张海峰, 张伟 |
|
Regulation of Structure and Magnetic Properties of Fe98.5 -x B x Cu1.5 Nanocrystalline Alloys Based on B Content |
| ZHU Chunjian, LI Yanhui, ZHU Zhengwang, WU Licheng, ZHANG Haifeng, ZHANG Wei |
| 图2 Fe98.5 - x B x Cu1.5 (x = 12~18)快淬合金的DSC曲线 |
| Fig.2 DSC curves of melt-spun Fe98.5 - x B x Cu1.5 (x = 12-18) alloys (Tx1—onset temperature of the first crystallization peak, Tx2—onset temperature of the second crystallization peak) |
|