双峰分离非基面织构AZ31镁合金板材反常中温轧制变形行为及机理 |
| 吴泽威, 颜俊雄, 胡励, 韩修柱 |
|
Abnormal Rolling Behavior and Deformation Mechanisms of Bimodal Non-Basal Texture AZ31 Magnesium Alloy Sheet at Medium Temperature |
| WU Zewei, YAN Junxiong, HU Li, HAN Xiuzhu |
| 图5 不同织构AZ31镁合金板材中温轧制变形过程中的再结晶晶粒演化 |
| Fig.5 EBSD images and (0002) PF (insets) showing the evolution of recrystallized grains within AZ31 magnesium alloy sheets with different textures during rolling process at medium temperature (a1-a3) the first (a1), second (a2), and fourth (a3) passes for basal texture sheets (b1-b3) the first (b1), second (b2), and fifth (b3) passes for bimodal non-basal texture sheets |
|