双峰分离非基面织构AZ31镁合金板材反常中温轧制变形行为及机理 |
| 吴泽威, 颜俊雄, 胡励, 韩修柱 |
|
Abnormal Rolling Behavior and Deformation Mechanisms of Bimodal Non-Basal Texture AZ31 Magnesium Alloy Sheet at Medium Temperature |
| WU Zewei, YAN Junxiong, HU Li, HAN Xiuzhu |
| 图4 双峰分离非基面织构AZ31镁合金板材中温轧制样品微观结构特征的EBSD分析 |