双峰分离非基面织构AZ31镁合金板材反常中温轧制变形行为及机理 |
| 吴泽威, 颜俊雄, 胡励, 韩修柱 |
|
Abnormal Rolling Behavior and Deformation Mechanisms of Bimodal Non-Basal Texture AZ31 Magnesium Alloy Sheet at Medium Temperature |
| WU Zewei, YAN Junxiong, HU Li, HAN Xiuzhu |
| 图3 基面织构AZ31镁合金板材中温轧制样品微观结构特征的EBSD分析 |
| Fig.3 EBSD analyses of microstructural characteristics of AZ31 magnesium alloy sheets with initial basal texture after the first (a1-a3), second (b1-b3), and fourth (c1-c3) passes of rolling at medium temperature (ET—extension twin, CT—compression twin, ST—secondary twin, HAGB—high angle grain boundary, LAGB—low angle grain boundary) (a1-c1) IPFs (a2-c2) grain boundary (GB) maps (a3-c3) grain orientation spread (GOS) maps |
|